SILVER PLATE ANTIQUING PROCESS

STEP 1

Components must be free from grease

STEP 2

Water wash to obtain a wetting condition

STEP 3

Immerse in Blackfast 183 until silver reaches a grey/black colour, not jet black. Dilution 1:1 with water or use neat if speed is important. Dwell time 5-10 minutes.

If speed is important, heat the solution up to 50ÂșC.

STEP 4

Water rinse

STEP 5

Dry components – methods available:
i) maize
ii) oven dry
iii) hot air

STEP 6

Relieve components if a contrasting effect is required – methods available:
i) rotary vibrating machine
ii) typhoon barrel
iii) manual clean with abrasive paper/cloth
iv) polish using a rotary bench polishing machine

STEP 7

Lacquer finish if required

APPLICATION DATA SHEETS

View complete technical information on how to effectively apply the various relevant solutions for your blacking production line.

SAFETY DATA SHEETS

Information for the safe handling of both Supplied (Concentrated) and Working (Diluted) Solutions.

SOLUTION STRENGTH TESTS

In each of the guides on this page, you’ll find testing processes based on proven tests for checking and adjusting the strength of our solutions

knowledge centre

Our knowledge centre is the hub for troubleshooting tips; answers to frequently asked questions; interesting information and the latest updates.

GOT A QUESTION?

We are here to help. Please contact us should you require more information or would like to book a demonstration. Telephone 020 8339 7370.

Get in touch